Read first-layer signals
قراءة إشارات الطبقة الأولى
A visual guide to identifying a too-high, too-low, and dependable first layer.
The problem
The first layer is separating, scraping, or inconsistent.
Why it happens
Bed condition, nozzle distance, leveling, and material preparation can all affect the first lines.
How to fix it
Watch a compact first-layer test, stop early when it is clearly wrong, and adjust one relevant variable.
Settings to try
Use a slow first layer Review the bed mesh Keep the build surface clean